Thermanit 617 TIG rod
Classifications high-alloyed
EN ISO 18274: AWS A5.14:
S Ni 6617 (NiCr22Co12Mo9) ERNiCrCoMo-1
Characteristics and field of use
Resistant to scaling up to 1100 °C (2012 °F), high temperature resistant up to 1000 °C (1832 °F).
High resistance to hot gases in oxidizing resp. carburizing atmospheres. For joining and surfacing
applications with matching and similar heat resistant steels and alloys.
Marks (rods0nly)
2.4627 / ERNiCrCoMo-1
Base materials
TüV-certified parent metal
1.4859 – UNS N08810 – GX10NiCrSiNb32-20
1.4876 – Alloy 800 – UNS N08800 – X10NiCrAlTi32-20
1.4958 – Alloy 800 H – UNS N08810 – X5NiCrAlTi31-20
2.4851 – Alloy – 601 – UNS N06601 – NiCr23Fe
2.4663 – Alloy 617 – UNS N06617 – NiCr23Co12Mo
Typical composition of welding rod (Wt-%)
C Si Mn Cr Mo Ni Co AI Ti Fe
0.05 0.1 0.1 21.5 9.0 Bal. 11.0 1.3 0.5 1.0
Mechanical properties of all-weld metal
Heat Treatment Yield strength
0.2%
Tensile
strength
Elongation
(L0=5d0)
Impact values
in J CVN
MPa MPa % +20°C:
AW 450 700 30 60
Operating data
Polarity = – Shielding gas (EN ISO 14175):
I1
Dimensions (mm)
1.6 2.0 2.4 3.2
Approvals and certificates
TüV (6845.)