Thermanit 35/45 Nb德國蒂森焊絲
Thermanit 35/45 Nb TIG rod
Classifications high-alloyed
EN ISO 18274:
S Ni Z (NiCr36Fe15Nb0.8)
Characteristics and field of use
Resistant to scaling up to 1180 °C (2156 °F).For joining and surfacing work0n matching/similar
heat resistant cast steel grades
Marks (rods0nly)
35 45 Nb / Ni 6701 mod.
Base materials
GX45NiCrNbSiTi45-35
Typical composition of welding rod (Wt-%)
C Si Mn Cr Ni Nb
0.42 1.5 1.0 35.0 45.5 0.8
Mechanical properties of all-weld metal
Heat Treatment Yield strength
0.2%
Tensile
strength
Elongation
(L0=5d0)
Impact values
in J CVN
MPa MPa %
AW 450 450
Operating data
Polarity = – Shielding gas (EN ISO 14175):
I1
Dimensions (mm)
2.0 2.4 3.2